Sprache
:
![]()
Neopentyl glycol diglycidyl ether YLD-6009, CAS 17557-23-2. It is colorless transparent liquid, no irritating odor.
YLD-6009 contains two epoxy groups within the molecule. It can form chain and network structure when curing.YLD-6009 is mainly used as the active diluent of epoxy resin, which can reduce the reactivity of epoxy resin and curing agent under the same temperature condition. It is widely used in, composites, anticorrosive coatings, solvent-free coatings, laminates, adhesives, transparent epoxy system LED and electrician's casting and molding epoxy system.
![]()

![]()
|
Item |
YLD-6009 |
|
Appearance |
Transparent liquid |
|
Color, APHA |
Max. 40 |
|
Viscosity, mpa.s 25°C |
10-25 |
|
EEW, g/eq |
136-148 |
|
Hydrolyzable Chloride,% |
Max. 0.2 |
|
Inorganic Chlorine, mg/kg |
Max. 20 |
|
Water,% |
Max. 0.1 |
| Color, (G) | ≤3.0 |
| EEW, g/eq | 170-190 |
| Viscosity, cps@25°C | H-K |
| Hy-Cl, ppm | ≤1000 |
![]()
![]()
Store in well-ventilated area. Keep away from flames and direct sunlight. Close the cap tightly immediately after use.
All safety information is provided in the Material Safety Data Sheet.
![]()
At least 12 months from the date of manufacture in the original packing in ambient temperatures.
![]()
Drum package.